AISI 4340, 4130 etc., Thin Dense Chrome plating & Hydrogen Embrittelment

Q. After applying TDC is it necessery to bake it to avoid Hydrogen Embrittelment and if so are the parameters of the bake similar to Hard chrome plating, i.e. 375°F for 12hrs?

A. Yes, you must bake after TDC plating, especially if the base material is a ferrous alloy. The potential for embrittlement due to the interaction between atomic hydrogen and the ferrous metallic atomic structure, is the same in TDC as in standard hexavalent hard chrome plating. Bake parameters are established to affect a specific type of steel and tensile strength. As the strength of the steel goes up, so does its susceptibility to Hydrogen embrittlement. A 12 hr. bake at 375oF is required for low alloy, high strength steels 220 ksi (220,000 psi) and above.

RT

 

 

 


The information contained in this site is provided for your review and convenience. It is not intended to provide legal advice with respect to any federal, state, or local regulation.
You should consult with legal counsel and appropriate authorities before interpreting any regulations or undertaking any specific course of action.

Please note that many of the regulatory discussions on STERC refer to federal regulations. In many cases, states or local governments have promulgated relevant rules and standards
that are different and/or more stringent than the federal regulations. Therefore, to assure full compliance, you should investigate and comply with all applicable federal, state and local regulations.